dc.description.abstractDevido à baixa retenção mecânica e ausência de ligações químicas de Zircónia, as facetas ultrafinas monolíticas de Zircónia versus outros tipos de cerâmica, estão mais sujeitos ao fracasso por falha adesiva. Para ultrapassar este inconveniente, vários tratamentos de superfície foram propostos para aumentar a força de ligação entre Y-TZP e o cimento resinoso. As técnicas de tratamento de superfície podem alterar a estrutura cristalina da cerâmica e fragiliza-las. O objetivo do estudo é de avaliar a adesão entre Y-TZP e o cimento resinoso usando diferentes tratamentos de superfície e avaliar quais as técnicas que incrementam a força de ligação com menos danos à estrutura. A pesquisa bibliográfica foi feita na base dados MEDLINE via Pubmed (Biblioteca Nacional de Medicina dos EUA National Institutes of Health). Pesquisa avançada foi selecionando e o filtro "dados associados" foram selecionados artigos dos últimos 10 anos. A partir desta revisão sistemática, podemos concluir que a abrasão do ar com Al2O3 é muito eficiente para aumentar a adesão mas aumenta muito o cisalhamento da superfície. Tratamento com Er:YAG laser pode constituir uma boa alternativa e parece provocar menos danos na estrutura em comparação ao ar abrasão, mas não é tão eficiente. Esta revisão sistemática aponta que o cimento ou o adesivo com MDP é importante para aumentar a adesão, criando uma ligação química. Outros tratamentos foram abordados nesta revisão, mas requerem mais estudos para serem crediveis.pt_PT
dc.description.abstractDue to the low mechanical retention and the lack of chemical bond of Zirconia, Ultrathin monolithic zirconia veneers are more subject to debond contrarily to other materials. To avoid this phenomenon, various surface treatments have been developed to evaluate the Shear Bond Strength between Y-TZP and resin cement and analyze the surface roughness after treatment. Those treatments could however alter the surface crystalline structure of the ceramic and weaken it. This study aims to evaluate the Shear Bond Strength between Y-TZP, and resin cement using different surface treatments and evaluate which one of these technics increases the bond strength with less fracture damage. Bibliographic research was carried out in the MEDLINE database via PubMed (US National Library of Medicine National Institutes of Health). Advanced research selecting the filter "associated data" was done including articles from the last 10 years. From this systematic review, we can notice that Air Abrasion with Al2O3 is very efficient to increase bonding but has increased a lot the surface roughness. Laser treatment with Er:YAG can be a good alternative and seems to be less traumatic than Air abrasion but not as efficient. This systematic review points that MDP containing resin is very important to increase bonding by creating a chemical bond. Other treatments have been addressed in this review but need more studies.pt_PT
dc.language.isoporpt_PT
dc.rightsinfo:eu-repo/semantics/openAccesspt_PT
dc.subjectZirconia OR zirconium OR Y-TZP AND Bond strengthpt_PT
dc.subjectZirconia)OR Zirconium AND Y-TZP AND Surface Treatmentpt_PT
dc.subjectZirconia veneer AND adhesionpt_PT
dc.subjectUltrathin veneerpt_PT
dc.titleDifferents surface treatments to increase bonding of ultrathin monolithic zircon veneers.pt_PT
dc.typeinfo:eu-repo/semantics/masterThesispt_PT
dc.identifier.tid202780805pt_PT
thesis.degree.nameMestrado em Medicina Dentáriapt_PT


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record